https://www.avient.com/products/fiber-line-engineered-fiber-solutions/fiber-line-performance-enhancing-processes
Gordon Glass™ Archery Bow Limbs
OnForce™ Long Glass Fiber Reinforced Polypropylene Composites
Long Glass Fiber Reinforcement
https://www.avient.com/products/polymer-additives/fiber-additives
OnForce™ Long Glass Fiber Reinforced Polypropylene Composites
Long Glass Fiber Reinforcement
CORE™ Plastisol Adhesives
https://www.avient.com/products/polymer-colorants/high-temperature-color-concentrates
OnForce™ Long Glass Fiber Reinforced Polypropylene Composites
Long Glass Fiber Reinforcement
CORE™ Plastisol Adhesives
https://www.avient.com/products/advanced-composites/short-long-fiber-formulations
OnForce™ Long Glass Fiber Reinforced Polypropylene Composites
Long Glass Fiber Reinforcement
CORE™ Plastisol Adhesives
https://www.avient.com/products/engineered-polymer-formulations/chemical-corrosion-resistant-formulations
OnForce™ Long Glass Fiber Reinforced Polypropylene Composites
Long Glass Fiber Reinforcement
CORE™ Plastisol Adhesives
https://www.avient.com/idea/could-polyketone-be-next-generation-nylon-alternative
The charts above compare 30% short glass-fiber filled samples and show a noticeable difference in the moisture uptake behavior of PK versus to PA6 & PA66.
40% Glass-Filled Resin
How well does this material work with adhesives for bonding?
https://www.avient.com/knowledge-base/case-study/lawn-and-garden-maker-adds-appeal-profitability?ind[]=6596
It required a high temperature and a strong injection pressure to bond to the acrylonitrile-butadienestyrene (ABS) substrate, which caused the resin to deform.
Product developers reported that they needed a better TPE to provide superior bonding performance with ABS without requiring high temperature and pressure during 2K molding.
Avient recommended an OnFlex™-S multicomponent TPE, which offers excellent adhesion to ABS and can be molded at lower temperatures and injection pressures than competitive products.
https://www.avient.com/knowledge-base/case-study/lawn-and-garden-maker-adds-appeal-profitability?pname[]=10744
It required a high temperature and a strong injection pressure to bond to the acrylonitrile-butadienestyrene (ABS) substrate, which caused the resin to deform.
Product developers reported that they needed a better TPE to provide superior bonding performance with ABS without requiring high temperature and pressure during 2K molding.
Avient recommended an OnFlex™-S multicomponent TPE, which offers excellent adhesion to ABS and can be molded at lower temperatures and injection pressures than competitive products.
https://www.avient.com/knowledge-base/case-study/lawn-and-garden-maker-adds-appeal-profitability?rtype[]=1124
It required a high temperature and a strong injection pressure to bond to the acrylonitrile-butadienestyrene (ABS) substrate, which caused the resin to deform.
Product developers reported that they needed a better TPE to provide superior bonding performance with ABS without requiring high temperature and pressure during 2K molding.
Avient recommended an OnFlex™-S multicomponent TPE, which offers excellent adhesion to ABS and can be molded at lower temperatures and injection pressures than competitive products.
https://www.avient.com/sites/default/files/resources/Novel_Thermoplastic_Elastomers_with_Universal_Bonding_Characteristics.pdf
This is because overmolding eliminates
the traditional bonding process which requires adhesives and primers for bonding and instead allows the
surface of an article of complicated design to be conveniently covered.
For
example, a TPE that can bond to PC does not bond to PP, vice versa.
The bonding characteristics of TPE-2 materials to all the substrates
were adhesive in nature.